PostPosted: Sun May 06, 2018 1:44 am 
Offline
Newly registered Member

Joined: Wed Feb 11, 2015 8:07 pm
Posts: 16
Has thanked: 13 times
Been thanked: 2 times
Hi guys,

I've had very little experience with protecting garden furniture and am really confused as to what to use exactly..oil/stain/paint etc

The Picnic table is new and made from Swedish Redwood, pressure​ ​treatment​ ​Tanalith​ ​E.

I would very much like to be able to see the grain after treatment and a slight satin sheen would be nice too.

So would very much appreciate advise on what best to use..brands and links most welcome lol

Edit : Just to add the Picnic Table has not been painted/stained/oiled where I'm buying it from.


Share on FacebookShare on TwitterShare on DiggShare on DeliciousShare on Google+
Top
 Profile  
Reply with quote  
PostPosted: Mon May 07, 2018 10:56 pm 
Offline
Senior Member

Joined: Thu Apr 14, 2011 7:33 pm
Posts: 3825
Location: Dundee, Scotland.
Has thanked: 728 times
Been thanked: 802 times
:welcome:

Howdy Silver. Oil is the best "preservative". Teac oil or something like this http://www.liberon.co.uk/product/garden-furniture-oil/. Not sure what trousers/skirt you should wear to figure out if the bench is not giving out the oil though. Oil as often as you can and protect during the winter.

Also check this company https://www.osmouk.com/ for any exterior oils. Their products are highly regarded.



For this message the author OchAye has received gratitude : Silver
Top
 Profile  
Reply with quote  
PostPosted: Tue May 08, 2018 12:28 am 
Offline
Newly registered Member

Joined: Wed Feb 11, 2015 8:07 pm
Posts: 16
Has thanked: 13 times
Been thanked: 2 times
Hi and thanks for the reply OchAye and welcome, I am looking into the osmo products and I see they have a range for decking. Since Decking would be high traffic I'm guessing the product would need to be even tougher than the normal garden furniture stuff ...I might be wrong though.

Right now I'm thinking between getting the Decking oil or their Natural Oil Woodstain



For this message the author Silver has received gratitude : OchAye
Top
 Profile  
Reply with quote  
PostPosted: Tue May 08, 2018 9:45 am 
Offline
Senior Member

Joined: Thu Apr 14, 2011 7:33 pm
Posts: 3825
Location: Dundee, Scotland.
Has thanked: 728 times
Been thanked: 802 times
The table being pressure treated may not take up that much - if any - stain. You lose nothing though by buying a stain oil, it will be more useful next year. Do not expect to just achieve the colour of the stain, the stain will be in addition to whatever colour you got and the result a bit darker than the wood you have etc. :-)



For this message the author OchAye has received gratitude : Silver
Top
 Profile  
Reply with quote  
PostPosted: Wed May 09, 2018 11:52 am 
Offline
Old School Chippie
User avatar

Joined: Mon Sep 12, 2011 4:27 pm
Posts: 5815
Location: Lancashire
Has thanked: 731 times
Been thanked: 1471 times
OchAye wrote:
The table being pressure treated may not take up that much - if any - stain. You lose nothing though by buying a stain oil, it will be more useful next year.

In the past when I did fencing and the like I always used to advise leaving it over the first winter before staining it as Tanalith E will inhibit even take-up of any applied finish. In other words you'll possibly get a blotchy finish. After the first winter this never seems to be a problem

_________________
"The person who never made a mistake, never made anything" - Albert Einstein

"I too will something make, And joy in the making" - Robert Bridges, 1844~1930



For this message the author Job and Knock has received gratitude : Silver
Top
 Profile  
Reply with quote  
PostPosted: Wed May 09, 2018 7:06 pm 
Offline
Senior Member

Joined: Tue Jul 05, 2016 7:16 pm
Posts: 105
Has thanked: 8 times
Been thanked: 14 times
Pressure treated timber needs a few month to cure before it is treated. Then use 3 coats of the treatment of your choice.



For this message the author Manc chippy has received gratitude : Silver
Top
 Profile  
Reply with quote  
PostPosted: Wed May 09, 2018 9:26 pm 
Offline
Newly registered Member

Joined: Wed Feb 11, 2015 8:07 pm
Posts: 16
Has thanked: 13 times
Been thanked: 2 times
Ok thanks everyone for the advice.

The company I purchased the table from advised me to just use a clear varnish, saying the treatment used would last 15 years.

However I think the best thing to do would be to wait at least a few months before using the exterior oil, then after that treat with oil yearly.


Top
 Profile  
Reply with quote  
Display posts from previous:  Sort by  
Post new topic Reply to topic  [ 7 posts ] 

 

 




Similar topics
   

Time zone: Europe/London [ DST ]


Who is online

Users browsing this forum: spottie and 4 guests


You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot post attachments in this forum

Search for:
Jump to:  
Visit Solent plastics


 

 

 

News News Site map Site map SitemapIndex SitemapIndex RSS Feed RSS Feed Channel list Channel list
ultimatehandyman privacy policy

Contact

 

Powered by phpBB® Forum Software © phpBB Group

phpBB SEO